Question · colour across substrates
Why one logo colour comes out different on steel, aluminium, plastic and fabric.
A colour reference describes printed ink on coated paper. None of these four surfaces is coated paper, and each one produces colour by a different mechanism, so the same reference drifts in four different directions. The drift is predictable once you know which mechanism you are dealing with.
The starting point
A colour chip is a sample of one process, not a target for all of them.
A Pantone number identifies a specific ink printed on a specific stock under controlled conditions. When it is used as a reference for anodised aluminium, it is being asked to describe something it was not designed to describe. That is not a failure of the supplier. It is a mismatch between the reference and the material.
Two consequences follow. The first is that a colour has to be approved separately on each surface, from a physical sample. The second is that some references are simply not reproducible on some materials, and the sooner that is said the cheaper it is.
Four mechanisms
The colour is made in four different places.
What matters is whether the colour sits on the surface, lives inside it, or is a change to the surface itself.
| Surface | How the colour is produced | What pulls it off reference |
|---|---|---|
| Powder-coated stainless | Pigment suspended in a cured polymer layer that covers the steel | Gloss level and film thickness change how light returns. A matte coat reads darker and flatter than the same pigment in a gloss coat, and two coat passes deepen it again. |
| Anodised aluminium | Dye absorbed into a porous oxide layer and sealed inside it | The colour lives under the surface, so oxide thickness and alloy both shift it, and a light anodising gives a paler result than a dark one for the same dye. |
| Bare stainless, laser marked | No colour is added at all. The mark is a localised change in surface oxidation and texture. | It cannot reproduce a hue. What it produces is a tonal contrast against the metal, which is strong on brushed steel and weak on mirror, where a base layer is needed first. |
| Moulded plastic | Ink sitting on the polymer surface | Surface energy decides whether the ink wets and stays. Untreated polypropylene is the hard case, which is why plasma or flame pre-treatment is standard rather than optional, and why an untreated part fails weeks later. |
| Knitted fabric | Ink absorbed into the fibres rather than resting on top | The weave scatters light, so the same ink reads lighter and less saturated. Fine detail fills in, and washing relaxes the knit, which changes apparent coverage. |
What actually decides a match
Three variables, and only one of them is the ink.
The substrate lot. Two batches of powder coat or anodising can differ before any ink touches them, especially at the lighter end of the range. Where a colour has to hold across a programme, the coat or anodising batch should be held too.
The ink batch. Mixed ink drifts more than factory-packed ink, so a multi-item range is better run from a single batch than from four mixes made a fortnight apart.
The cure. Under-cured ink is lighter and less fast; over-cured ink can yellow or lose adhesion. Cure parameters belong in the record, not in somebody's memory, because the next run has to repeat them.
There is a fourth factor that surfaces only after delivery. Two colours can match under one light and diverge under another, which is called metamerism. Approval under a daylight standard such as D50 avoids it, and approving under office lighting invites it, because the warm LED lighting of a retail shelf is a different test again.
Control
How a range is kept consistent.
- A physical drawdown per surface, judged together Each material gets its own proof, and the proofs are compared side by side under one light rather than one at a time. A colour approved in isolation passes tests it should fail.
- The approved drawdown becomes the reference Not the Pantone number, and not a photograph. The signed physical sample is what the run is measured against, because it carries the substrate's contribution that a colour chip cannot.
- One specification covering every item Substrate, ink reference, coat or anodising batch, cure parameters and the acceptance standard, applied to all items in the programme. Without it, four suppliers will each deliver something defensible and nothing that matches.
- Verification that survives handling Cross-hatch or tape-pull for adhesion, a wash test for textiles, and a side-by-side visual check under the agreed light. Adhesion is the one that matters most, because a colour that matches today and lifts in three weeks is worse than a colour that is slightly off.
What to settle at brief stage
Choices that travel well
- One or two colours, solid, with no fine gradients
- Laser marking on bare metal, where a tonal mark is acceptable
- Darker colours, which hide substrate variation better
- The same substrate across every item in the set
Choices that fight the material
- Full-colour process printing on knitted fabric
- A specific hue produced by laser marking
- Fluorescent or metallic references on plastic
- Very light pastels across mixed coat batches
A programme that ran the same logo across four substrates is written up in the reference delivery, including what failed first on each surface. The decoration routes themselves, surface by surface, are set out under custom drinkware.
Not sure your colour will survive the material?
Send the artwork and the items. We will tell you which references are reproducible on which surface before anything is sampled.